PropertiesCorrosion Resistance

Pitting potential measurement: JIS G-0577:2005

Conditions

  • Solution: 5% NaCl, 25 ⁰C
  • Counter electrode: Platinum
  • Reference electrode: Ag/AgCl
  • The tested surface was fully immersed in test solution for 2 h
  • The test was conducted by potentiokinetic method from natural electrode potential to 1 mA/cm2 of anodic current density
  • Potential sweeping velocity: 1mV/s
  Ecorr
(mV vs Ag/AgCl)
Log Jcorr
(mA/cm2)
Stainless Steel -106 -2.54
Ceramic Coating UNALTERED